Successful dosing processes necessitate meticulous product preparation, and AusOptic is pleased to present the complete range of planetary mixers manufactured by THINKY.
The THINKY Corporation’s ‘Thinky Mixer’ combines two rotations and a revolution to mix and degas materials simultaneously, revolutionising material processing. THINKY offers compact desktop units for labs and large models for mass production, showcasing its innovative technology and expertise in building a foundation for production environments.
The principle of rotation / revolution, two powerful centrifugal forces orbit harmoniously and also rotate on their own axis. The deaeration phenomenon guarantees a bubble-free result.
Yellow acrinol powders are uniformly dispersed to create a solid yellow colour cream with a smooth feel when applied.
Fluorescent powders with a higher specific gravity are uniformly dispersed without sedimentation.
The fluorescent material is uniformly dispersed with no sedimentation throughout the low-viscosity silicone resin.
No bubbles. Uniformity mixed.
Four types of materials are uniformly mixed to a smooth cream consistency.
Smooth Surface. No bubbles.
Two part resin and white alumina powder are uniformly mixed to a solid green colour.
No lumps. Powders turn into a uniformly mixed paste.
Applications | THINKY Mixer | Viscosity, Density, Particle Volume or Size |
||
1 | Ceramic (10 V%) | Dispersion Defoaming | ARE-250 2 minutes | Barium Titanate – 6.02g/cm3 Micron particle, 10 volume %, (Total 120g) |
2 | Nano Ceramic (70 V%) | Dispersion Defoaming | ARE-250 3 minutes | Aluminum oxide – 0.5µm Nano particle, 3.97g/cm3 50-70 volume % |
3 | 2 part Epoxy | Mixing Defoaming | ARE-250 20 seconds | Epoxy Part A: 3000-6000 poise Part B: 0.3-0.7 poise |
4 | Carbon Nano Fiber (10V%) | Dispersion | ARE-250 3 minutes | CNF-10 volume % Nano particle, Fiber |
5 | Carbon Black 2 part silicone (20 wt%) | Dispersion Defoaming | ARV-310 1 minutes/ ARE-250 8 minutes | Nano Carbon Black 20wt% (50V%) Nano particle (Total 120g) |
6 | Silicone Potting Compounds | Mixing Defoaming | ARV-310 3 minutes | Part A: 4000-8000 poise Part B: 200-700 poise (Total 10g) |
7 | Precious metal paste | Dispersion Defoaming | ARV-310 / ARE-250 from 30 sec. to 1 min | General silver filled condudctive epoxy / Jar and syringe application Highly dense metal powder |
8 | Carbon NanoTube (1-2 wt%) | Dispersion | ARV-310 6 min | CNT – 1-2 wt% Nano particle tube |
9 | Zinc Oxide(10 V%) | Dispersion Defoaming | ARE-250 6 min | ZnO 10 volume % petroleum Jelly 0.85, Zinc Oxide 5.76 |
10 | LCD ODF sealant (10V%) | Dispersion Deforming | ARV-5000 TWIN | Au Ball 10 volume % sealant 400,000cP, Au ball 3µ |
11 | Printing Ink | Degas | ARV-5000 | Solvent Ink 450g |
12 | Viscous Epoxy | Defoaming | ARE-250250AD-EFD-3×6 | Epoxy 828 2.5cc in EFD 3cc Syringe |
13 | Alumina | Dispersion Defoaming | ARV-5000 | Aluminum oxide – 20 volume % Silicone 3000cP |
14 | LED Phosphor | Dispersion Defoaming | ARV-310+ Syringe Loader | Phosphor 10 wt% Slicone 10,000cP 20g |
15 | Viscous Epoxy | Defoaming | ARV-310 + Syringe Loader | Various Epoxy sample |
16 | Talc | Dispersion Defoaming | ARE-250 | Silicone 60g – 30wt% Silicone 10,000cP |
17 | CNF (1%wt) | Dispersion Defoaming | ARV-310 6min | CNF 1%wt |
18 | Suspension | Particle Reduction | ARE-250 3min | Phenytoin as API |